I. Common causes affecting casting surface finish
1. Raw materials, such as the shape of the moulding sand. Round, square and triangular grains behave differently: triangular sand is the poorest because of its large gaps (with resin sand it also increases resin addition and gas evolution, which can cause blowholes if venting is poor), while round sand is the best. For coal-dust sand, the sand mix (strength and moisture) also strongly affects appearance; for CO2 hardened sand, the coating is the main factor.
2. Material. If the chemical composition of the casting is out of balance, for example with low manganese, porosity and a coarse surface structure can result.
3. Gating system. An poorly designed gating system can also cause porosity, and in severe cases misruns or incomplete castings.An inadequate slag trapping system allows slag to enter the cavity and produce slag inclusions.
4. Slag formation. If slag is not fully removed from the molten iron, or is not held back during pouring, slag enters the cavity and slag holes are inevitable.
5. Human factors. Carelessness, sand left in the mould at closing, insufficient ramming, or an unreasonable sand mix with low strength can all produce sand holes in the casting.
6. Excessive sulphur and phosphorus can cause cracking. These are all points that must be watched during production in order to guarantee casting quality.
The causes above are only a small part of the picture. Casting production is highly variable and complex, and problems arise frequently in practice; sometimes a single fault can take a long time to trace.
II. Three main factors affecting the surface roughness of gray cast iron
Surface roughness is an important measure of the surface quality of gray iron parts. It directly affects both the appearance of the part and the assembly quality and service life of the machine. This article examines how to improve surface roughness from three angles: the machine tool, the cutting tool and the cutting parameters.
Poor machine rigidity, low spindle accuracy, insecure mounting and excessive clearances between components all affect the surface roughness of gray iron parts.
For example, if spindle runout is 0.002 mm (2 microns), it is theoretically impossible to machine a workpiece with roughness below 0.002 mm, although a Ra 1.0 surface is generally achievable. Gray iron is a casting and cannot be finished to a high surface quality as readily as steel, and poor machine condition makes roughness harder to guarantee.
Machine rigidity is normally fixed at the factory and cannot be changed. Beyond rigidity, spindle clearance can be adjusted and bearing accuracy improved to reduce machine clearances, providing some assurance of better surface roughness when machining gray iron parts.
Selection of tool material
When tool and workpiece materials have high mutual affinity, the workpiece tends to adhere to the tool, forming built-up edge and scaly surface defects; severe adhesion and friction increase surface roughness. When machining gray iron, carbide inserts struggle to reach Ra 1.6 and tool life suffers even if they do, whereas CBN tools such as BNK30, with a low friction coefficient, excellent high-temperature stability and wear resistance, readily achieve Ra 1.6 at cutting speeds several times higher than carbide, with tool life tens of times longer and a markedly brighter surface.
Selection of tool geometry
Among tool geometry parameters, the entering angle has the greatest influence on surface roughness.The main parameters are the entering angle Kr, minor cutting edge angle Kr' and corner radius re. Smaller entering and minor angles reduce the height of residual area on the machined surface and thus lower roughness; a smaller minor angle reduces roughness but can induce vibration, so it must be chosen according to machine rigidity. Within the limits of system stiffness, increasing re lowers roughness, so reducing Kr and Kr' and increasing the corner radius all reduce residual area height and surface roughness.
As tooling engineers put it,It is recommended to select the corner radius according to workpiece rigidity and roughness requirements: with good rigidity a larger radius improves both efficiency and surface finish, whereas boring, slender shafts and thin-walled parts with poor system stiffness usually require a smaller corner radius.
Tool wear
Tool wear proceeds in three stages.Initial wear, normal wear and severe wear. Once a tool enters the severe wear stage, flank wear rises sharply, the system becomes unstable, vibration increases and surface roughness varies widely.
In gray iron machining many parts are produced in batches with demanding consistency and productivity requirements, so many shops replace tools before the third stage, a practice known as forced tool change. Shops run repeated tests to find the critical point that preserves surface roughness and dimensional accuracy without hurting overall productivity.
Casting defects in the part itself, an unsuitable cutting fluid and the choice of machining method can also affect surface roughness.
As tooling engineers put it,In turning, milling or boring gray iron, and where machine and cutting parameters allow, CBN tools can achieve Ra 0.8, though with some impact on tool life; the choice depends on actual machining conditions. Besides machine tool, cutting tool and cutting parameters, the cutting fluid, the gray iron part itself and the machining method also influence surface roughness.
Since surface roughness has a fairly direct effect on the performance of machine parts, and the factors influencing it in production are many, all relevant factors should be considered together and economically appropriate roughness requirements set according to actual need.
Service Hotline